OBJECTIVES: To assess the effect of ozone gas on the mechanical properties of different classes of dental adhesives. METHODS: Extracted molars were sectioned perpendicularly to their long axis for obtaining dentin slices to be bonded with one of the following adhesives: Prime&Bond NT (Dentsply), Excite (Ivoclar-Vivadent), Syntac/Heliobond (Ivoclar-Vivadent) and Silorane System Adhesive (3 M-ESPE). Prior to bonding, the slices were sectioned in two halves: one was treated with ozone gas for 120 s (4.2g/m3; HealOzone, KaVo) and the other served as control. The Vicker's hardness (VH), elastic modulus (E), elastic work (We/Wtot) and the creep (Cr) of the materials were measured with an automatic micro hardness indenter (Fischer) 30 min and 24 h after bonding procedure. Data were analyzed with the multivariate ANOVA followed by the Tukey's test and partial eta-squared statistics. RESULTS: The adhesive and the time of testing were significant factors affecting the investigated parameters (p<0.001; etap2>or=0.06). Dentin treatment, though significant, exerted a minimal effect on mechanical properties (etap2
Magni, E., Ferrari, M., Hickel, R., Huth, K.C., Ilie, N. (2008). Effect of ozone gas application on the mechanical properties of dental adhesives bonded to dentin. DENTAL MATERIALS, 24(10), 1428-1434 [10.1016/j.dental.2008.06.004].
Effect of ozone gas application on the mechanical properties of dental adhesives bonded to dentin
FERRARI M.;
2008-01-01
Abstract
OBJECTIVES: To assess the effect of ozone gas on the mechanical properties of different classes of dental adhesives. METHODS: Extracted molars were sectioned perpendicularly to their long axis for obtaining dentin slices to be bonded with one of the following adhesives: Prime&Bond NT (Dentsply), Excite (Ivoclar-Vivadent), Syntac/Heliobond (Ivoclar-Vivadent) and Silorane System Adhesive (3 M-ESPE). Prior to bonding, the slices were sectioned in two halves: one was treated with ozone gas for 120 s (4.2g/m3; HealOzone, KaVo) and the other served as control. The Vicker's hardness (VH), elastic modulus (E), elastic work (We/Wtot) and the creep (Cr) of the materials were measured with an automatic micro hardness indenter (Fischer) 30 min and 24 h after bonding procedure. Data were analyzed with the multivariate ANOVA followed by the Tukey's test and partial eta-squared statistics. RESULTS: The adhesive and the time of testing were significant factors affecting the investigated parameters (p<0.001; etap2>or=0.06). Dentin treatment, though significant, exerted a minimal effect on mechanical properties (etap2I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.
https://hdl.handle.net/11365/34705
Attenzione
Attenzione! I dati visualizzati non sono stati sottoposti a validazione da parte dell'ateneo