Objective: To assess the efficacy of dedicated finishing/polishing systems on roughness and gloss of VITA Suprinity and IPS e.max CAD. Method: A total of 24 blocks of Suprinity and 24 of e.max were cut into a wedge shape using an InLab MC-XL milling unit. After crystallization, the 24 Suprinity wedges were divided into four subgroups: group A.1: Suprinity Polishing Set Clinical used for 30 seconds and group A.2: for 60 seconds; group A.3: VITA Akzent Plus Paste; and group A.4: spray. The 24 e.max wedges (group B) were divided into four subgroups accorDing to the finishing procedure: group B.1: Optrafine Ceramic Polishing System for 30 seconds and group B.2: for 60 seconds; group B.3: IPS e.max CAD Crystall/ Glaze paste; and group B.4: spray. After finishing/ polishing, gloss was assessed with a glossmeter and roughness evaluated with a profilometer. Results were analyzed by applying a two-way analysis of variance for gloss and another for roughness (a=0.05). One specimen per each subgroup was observed with a scanning electron microscope.

Vichi, A., Fabian Fonzar, R., Goracci, C., Carrabba, M., Ferrari, M. (2018). Effect of finishing and polishing on roughness and gloss of lithium disilicate and lithium silicate zirconia reinforced glass ceramic for CAD/CAM systems. OPERATIVE DENTISTRY, 43(1), 90-100 [10.2341/16-381-L].

Effect of finishing and polishing on roughness and gloss of lithium disilicate and lithium silicate zirconia reinforced glass ceramic for CAD/CAM systems

Vichi A.
;
Fabian Fonzar R.;Goracci C.;Carrabba M.;Ferrari M.
2018-01-01

Abstract

Objective: To assess the efficacy of dedicated finishing/polishing systems on roughness and gloss of VITA Suprinity and IPS e.max CAD. Method: A total of 24 blocks of Suprinity and 24 of e.max were cut into a wedge shape using an InLab MC-XL milling unit. After crystallization, the 24 Suprinity wedges were divided into four subgroups: group A.1: Suprinity Polishing Set Clinical used for 30 seconds and group A.2: for 60 seconds; group A.3: VITA Akzent Plus Paste; and group A.4: spray. The 24 e.max wedges (group B) were divided into four subgroups accorDing to the finishing procedure: group B.1: Optrafine Ceramic Polishing System for 30 seconds and group B.2: for 60 seconds; group B.3: IPS e.max CAD Crystall/ Glaze paste; and group B.4: spray. After finishing/ polishing, gloss was assessed with a glossmeter and roughness evaluated with a profilometer. Results were analyzed by applying a two-way analysis of variance for gloss and another for roughness (a=0.05). One specimen per each subgroup was observed with a scanning electron microscope.
2018
Vichi, A., Fabian Fonzar, R., Goracci, C., Carrabba, M., Ferrari, M. (2018). Effect of finishing and polishing on roughness and gloss of lithium disilicate and lithium silicate zirconia reinforced glass ceramic for CAD/CAM systems. OPERATIVE DENTISTRY, 43(1), 90-100 [10.2341/16-381-L].
File in questo prodotto:
File Dimensione Formato  
Vichi Oper Dent 2018.pdf

non disponibili

Tipologia: PDF editoriale
Licenza: NON PUBBLICO - Accesso privato/ristretto
Dimensione 326.51 kB
Formato Adobe PDF
326.51 kB Adobe PDF   Visualizza/Apri   Richiedi una copia

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11365/1196976