Background: In this study, we assess the effect produced on roughness and gloss of fullbody bulk-fill materials by different finishing and polishing systems. Methods: Four full-body bulkfill materials were tested: SonicFill2 (SF), Filtek Bulk Fill Posterior Restorative (FB), Tetric EvoCeram bulk-fill (EC), and Fill-Up! (FU). Sixty discs per material (2 mm in thickness and 7 mm in diameter) were obtained and randomly assigned (n = 15) to four finishing and polishing methods: Sof-Lex Spiral Wheels (SW), HiLusterPLUS (HL), Astropol (AP), and Opti1Step (OS). Surface roughness and gloss were then measured. Results: For roughness, material and surface treatment were significant factors (p < 0.001) with SF = FB = EC < FU and AP < SW < HL = OS. Material and surface treatment had a significant effect also on gloss (p < 0.001), with SF > FB = EC > FU and SW > AP > HL > OS. Conclusions: The tested combinations of bulk-fill and polishing systems provided clinically acceptable results with regard to roughness, while the outcome was poor for gloss. Multistep finishing/polishing systems were able to produce smoother surfaces on full-body bulk-fill materials compared to simplified ones.

Paolone, G., Moratti, E., Goracci, C., Gherlone, E., Vichi, A. (2020). Effect of finishing systems on surface roughness and gloss of full-body bulk-fill resin composites. MATERIALS, 13(24), 1-9 [10.3390/ma13245657].

Effect of finishing systems on surface roughness and gloss of full-body bulk-fill resin composites

Goracci C.;
2020-01-01

Abstract

Background: In this study, we assess the effect produced on roughness and gloss of fullbody bulk-fill materials by different finishing and polishing systems. Methods: Four full-body bulkfill materials were tested: SonicFill2 (SF), Filtek Bulk Fill Posterior Restorative (FB), Tetric EvoCeram bulk-fill (EC), and Fill-Up! (FU). Sixty discs per material (2 mm in thickness and 7 mm in diameter) were obtained and randomly assigned (n = 15) to four finishing and polishing methods: Sof-Lex Spiral Wheels (SW), HiLusterPLUS (HL), Astropol (AP), and Opti1Step (OS). Surface roughness and gloss were then measured. Results: For roughness, material and surface treatment were significant factors (p < 0.001) with SF = FB = EC < FU and AP < SW < HL = OS. Material and surface treatment had a significant effect also on gloss (p < 0.001), with SF > FB = EC > FU and SW > AP > HL > OS. Conclusions: The tested combinations of bulk-fill and polishing systems provided clinically acceptable results with regard to roughness, while the outcome was poor for gloss. Multistep finishing/polishing systems were able to produce smoother surfaces on full-body bulk-fill materials compared to simplified ones.
2020
Paolone, G., Moratti, E., Goracci, C., Gherlone, E., Vichi, A. (2020). Effect of finishing systems on surface roughness and gloss of full-body bulk-fill resin composites. MATERIALS, 13(24), 1-9 [10.3390/ma13245657].
File in questo prodotto:
File Dimensione Formato  
Paolone_Materials 2020.pdf

accesso aperto

Descrizione: Articolo
Tipologia: PDF editoriale
Licenza: Creative commons
Dimensione 631.23 kB
Formato Adobe PDF
631.23 kB Adobe PDF Visualizza/Apri

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11365/1196970